Phase transformations in an α2 titanium superalloy II. Effect of aging temperature on the phase composition and structure of the alloy

S. L. Demakov, L. S. Stepanov, V. D. Kibal'nik, A. A. Popov

Research output: Contribution to journalArticle

Fingerprint Dive into the research topics of 'Phase transformations in an α2 titanium superalloy II. Effect of aging temperature on the phase composition and structure of the alloy'. Together they form a unique fingerprint.

Chemical Compounds

Engineering & Materials Science

Physics & Astronomy