ПОВЫШЕНИЕ ИЗНОСОСТОЙКОСТИ ХРОМИСТЫХ ЧУГУНОВ ТЕРМИЧЕСКОЙ ОБРАБОТКОЙ

Resultado de pesquisa: Articlerevisão de pares

Resumo

The maximum abrasive wear resistance is provided by metal base from metastable retain austenite and martensite. Such a microstructure of chromium cast irons, 260Kh16M2 and 250Kh25MFT with different types of carbides - Cr7C3 and Cr23C6, is created by high-temperature quenching with heating to temperatures of 1125-1170 °C and cooling in oil or air. Austenite is transformed to disperse martensite on the working surface as a result of the abrasive particles impact during operation. It and carbides provide a high hardening level and working capacity of the cast irons secondary microstructure.
Título traduzido da contribuiçãoCHROME CAST IRONS WEAR RESISTANCE IMPROVING BY HEAT TREATMENT
Idioma originalRussian
Páginas (de-até)35-40
Número de páginas6
RevistaЛитейщик России
Número de emissão8
Estado da publicaçãoPublished - 2020

GRNTI

  • 53.49.00

Level of Research Output

  • VAK List

Impressão digital

Mergulhe nos tópicos de investigação de “ПОВЫШЕНИЕ ИЗНОСОСТОЙКОСТИ ХРОМИСТЫХ ЧУГУНОВ ТЕРМИЧЕСКОЙ ОБРАБОТКОЙ“. Em conjunto formam uma impressão digital única.

Citar isto