SUBSTANCE: invention can be used in microelectronic equipment with low currents and voltages, where switching is required in time intervals of 20 to 70 minutes at 10-150 °C. The resistive material contains silver sulfide, germanium sulfide, non-stoichiometric, stoichiometric arsenic sulfide and 7 atomic percent of carbon in the form of single-wall nanotubes according to the empirical formula: AgGe1+xAs1-x(S+CNT)3, where 0.4≤x≤0.6.
EFFECT: provision of electrical conductivity relaxation time from 4 to 18 seconds and electrical resistivity of 106-109 Ohm⋅m, in the temperature range of 10-150 degrees.
SUBSTANCE: invention can be used in microelectronic equipment with low currents and voltages, where switching is required in time intervals of 20 to 70 minutes at 10-150 °C. The resistive material contains silver sulfide, germanium sulfide, non-stoichiometric, stoichiometric arsenic sulfide and 7 atomic percent of carbon in the form of single-wall nanotubes according to the empirical formula: AgGe1+xAs1-x(S+CNT)3, where 0.4≤x≤0.6.
EFFECT: provision of electrical conductivity relaxation time from 4 to 18 seconds and electrical resistivity of 106-109 Ohm⋅m, in the temperature range of 10-150 degrees.
投稿的翻译标题 | RESISTIVE MATERIAL BASED ON GLASS CHALCOGENIDES WITH NANOTUBES: patent of invention |
---|---|
源语言 | Russian |
专利号 | 2614942 |
IPC | H01C 7/00 |
归档日期 | 31/12/2015 |
州 | Published - 31 3月 2017 |