ТЕХНОЛОГИЧЕСКИЕ ВОЗМОЖНОСТИ ПРОИЗВОДСТВА ЖЕЛЕЗОРУДНОГО АГЛОМЕРАТА С ИСПОЛЬЗОВАНИЕМ КОМБИНИРОВАННОГО ТОПЛИВА

科研成果: Article

摘要

For combined combustion of solid and gaseous fuel in layer of aglosicht it is required mixing and clogging of initial materials, their laying on grate, initial heating of layer under incendiary mountain and ignition of solid fuel of charge, supply of poor gas-air mixture with air consumption factor more than 3.5 through special gas-air distribution device. Initial mixture of gases passing through hot layer of agglomerate of upper horizon is heated to ignition temperature (450 - 600 °C) with formation of active combustion zone of gaseous fuel at temperature of 1100 - 1150 °C with the length of 40 - 60 mm. The generated heat provides additional heating of the upper horizons of the layer to the required sintering temperature of the charge materials. Industrial tests of the HGRPprocess design on the АК-50 machine are shown that when combined fuel is used in the layer, the redox conditions are equalized according to its height and width with the possibility of increasing the productivity of the machine by 30 - 35 %. When switching to a combined fuel agglomerate, there is a steady tendency to increase the blast furnace productivity by 10 - 14 % on average, and to reduce the specific coke consumption for cast iron production by 8 %.
投稿的翻译标题Technological capabilities of iron ore agglomerate production using combined fuel
源语言Russian
页(从-至)28-35
页数8
期刊Проблемы черной металлургии и материаловедения
4
Published - 2019

GRNTI

  • 53.00.00 METALLURGY

Level of Research Output

  • VAK List

指纹 探究 'ТЕХНОЛОГИЧЕСКИЕ ВОЗМОЖНОСТИ ПРОИЗВОДСТВА ЖЕЛЕЗОРУДНОГО АГЛОМЕРАТА С ИСПОЛЬЗОВАНИЕМ КОМБИНИРОВАННОГО ТОПЛИВА' 的科研主题。它们共同构成独一无二的指纹。